Description: Ivory burning legacy kaolin
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.50% | 0.02 | |
| TiO2 | 1.00% | 0.03 | |
| Al2O3 | 40.00% | 1.00 | |
| SiO2 | 44.00% | 1.87 | |
| Fe2O3 | 0.50% | 0.01 | |
| Cl | 13.25% | n/a | |
| Oxide Weight | 219.30 | ||
| Formula Weight | 252.80 | ||
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |