Ferro Frit CC-261

Alternate Names: Frit CC261

Description: Zinc frit

Oxide Analysis Formula Tolerance
ZnO 10.90% 1.00
Oxide Weight 81.40
Formula Weight 81.40

Notes

SiO2:Al2O3 ratio is 11.51
Alkalies: 5-15%
CaO 5-15%
MgO less than 5%
Al2O3 5-15%
B2O3 less than 5%
SiO2 over 50%

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.7
By Tony Hansen