Potclays Frit 2270

Alternate Names: 2270 Hvit zircon Boraks fritte, Potclays White Zircon Borax Frit

Description: White Zircon Frit

Oxide Analysis Formula Tolerance
CaO 5.47% 0.41
MgO 1.06% 0.11
ZrO2 12.38% 0.43
Na2O 6.06% 0.41
Al2O3 5.68% 0.24
B2O3 13.58% 0.83
SiO2 54.60% 3.85
ZnO 1.17% 0.06
Oxide Weight 423.87
Formula Weight 423.87

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3302-D
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.