P29 Frit

Alternate Names: P29 Bly-bi-silikat, Frit P29

Description: Lead alumina bilsilicate frit

Oxide Analysis Formula Tolerance
PbO 64.93% 1.00
Al2O3 2.55% 0.09
SiO2 32.52% 1.86
Oxide Weight 343.75
Formula Weight 343.75

Notes

Was available in Norway, manufacturer unknown. Info from http://www.potters.org/subject70375.htm

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Melting Range (C) 900-1100