Ochre

Description: From Ron Roy's MDT

Oxide Analysis Formula Tolerance
CaO 0.30% 0.04
MgO 0.10% 0.02
Al2O3 15.00% 1.00
SiO2 74.00% 8.37
Fe2O3 10.60% 0.45
Oxide Weight 680.00
Formula Weight 680.00

Related Information

Links

Materials Ochre
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.