Frit 1451

Description: Netherlands, Flanders area (Ferro?)

Oxide Analysis Formula Tolerance
Na2O 16.65% 1.00
B2O3 37.20% 1.99
SiO2 46.15% 2.86
Oxide Weight 372.37
Formula Weight 372.37

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy