Labradorite

Oxide Analysis Formula Tolerance
SiO2 53.00% 3.08
Al2O3 30.00% 1.03
Na2O 4.50% 0.25
CaO 12.00% 0.75
Oxide Weight 347.31
Formula Weight 347.31

Notes

Analysis provided is of a sample material from Madagascar.