March 2026: We are doing major upgrades to code here, please be patient regarding any issues. If any page is not working for a period of hours, please contact us. Thank you.
| Monthly Tech-Tip | Feb 14-15, 2026 - Major Server Upgrade Done | No tracking! No ads! |
Description: Calcined fireclay
| Oxide | Analysis | Formula | Tolerance |
|---|
| Materials |
Fireclay
|
| Typecodes |
Aggregate
Granular materials intended to impart raw and fired structural strength or thermal expansion properties to bodies or deliver special speckling effects in glazes. |
| URLs |
https://www.imerys.com/product-ranges/chamotte-ceramics
Chamotte information from Imerys Chamotte—also known as 'grog', 'firesand' or “fireclay”—is calcined clay containing a high proportion of alumina. It is produced by firing selected fire clays in a rotary kiln. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk