1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Vermiculite

Oxide Analysis Formula Tolerance
CaO 10.99% 0.26
Li2O 0.06% -
MgO 22.20% 0.74
Al2O3 7.96% 0.10
SiO2 49.00% 1.09
LOI 9.80%n/a
Oxide Weight 120.48
Formula Weight 133.57

Notes

Clay-making mineral of the ideal form (Mg, Ca)x(Si8-x Alx(Mg, Fe)6O20, 8H2O of varying typical analyses.
Hardness 1.6 Density 2.3-2.7 Water insoluble
Used principally in refractory materials for purposes of insulation.