Formula: Al2O3
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 100.00% | 1.00 | |
| Oxide Weight | 102.00 | ||
| Formula Weight | 102.00 | ||
Tabular alumina is made by holding calcined alumina powder just below its 2040C fusion temperature to recrystallize the normally flat crystals into hexagonal, elongated tablet-shaped ones up to 400 microns in size. It is possible to convert near 100% of the crystals and achieve a high chemical purity. The new crystals maintain the same hardness and density and have much better thermal shock resistance.
Tabular aluminas are useful in ceramics, electrical insulators, dielectrics and refractory applications. They are available in sizes from around 40 mesh down to 325 mesh.

This picture has its own page with more detail, click here to see it.
Online at Ebay.com apparently!
| Materials |
Alumina Hydrate
|
| Materials |
Alumina
|
| Materials |
Calcined Alumina
A high-purity Al2O3 used in technical ceramics, refractories, glazes, and bodies for its extreme hardness, high-temperature strength, and chemical stability. |
| Typecodes |
Alumina
Alumina products |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk