95 Magnesite

Oxide Analysis Formula Tolerance
CaO 1.40% 0.01
MgO 95.90% 0.99
Al2O3 0.50% -
SiO2 1.60% 0.01
Fe2O3 0.60% -
Oxide Weight 41.59
Formula Weight 41.59

Notes

Produced by crushing and screening of selective dead burned magnesite ores.
Available in 4 to 10 mesh sizes.

Produced at Resco Canada in Grenville, Quebec.

Related Information

Links

Materials Magnesite
Typecodes Refractory
Materials that melt at high temperatures. These are normally used for kiln bricks, furniture, etc. or for ceramics that must withstand high temperatures during service.