C-90 Magnesite

Oxide Analysis Formula Tolerance
CaO 1.50% 1.72
MgO 91.60% 145.81
Al2O3 1.59% 1.00
SiO2 4.00% 4.27
Fe2O3 0.81% 0.32
LOI 0.50%n/a
Oxide Weight 6,383.02
Formula Weight 6,415.09

Related Information

Links

Typecodes Refractory
Materials that melt at high temperatures. These are normally used for kiln bricks, furniture, etc. or for ceramics that must withstand high temperatures during service.