Stain 6031

Description: Deep Salmon (CrSnFe)

Notes

Old number: 331

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

Mechanisms

Glaze ColorGlaze must be zincless & have a whiting content of 12-15% (CaO 6.7-8.4%).