1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Stain (grey)

Description: Greys (ZrCoFeNi)

Notes

Made from mixtures of zirconium oxide together with oxides of cobalt, iron and nickel.

Color Range
-----------
Shades of grey ranging from yellowy brown to neutral.

Specific Gravity: 4.5-4.7
----------------

Stability/Kiln Atmosphere
-------------------------
Stable at temperatures up to over 1300C in an oxidizing to slightly reducing atmosphere.

Compatibility
-------------
Suitable for blending with most other types of ceramic colors.

Cost
----
Relatively low.

Note: This description is taken from information provided by Blythe Matthey and may or may not apply to stains of this family from other companies.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

Mechanisms

Glaze ColorDo not make grey shades by using small amounts of black since the dominant oxide in the formulation will impose its shade of color (e.g. blue from cobalt). It is better to use grey stain.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy