1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

SicoNide

Description: Silicon Nitride Powder

Notes

Purity as little as 0.04 Fe, 0.05 Al, 0.01 Ca, 0.3 C, 0.002 Halides, and 0.7 Oxygen.
Particle sizes available down to 20 microns.

Parmascand, the manufacturer, has a booklet on processing of Si3N4 materials. It covers slip preparation, casing, pressing, tape casting, binders, and sintering.