SA-85 Bauxite

Oxide Analysis Formula Tolerance
CaO 1.90% 0.01
MgO 96.28% 0.99
Al2O3 0.20% -
SiO2 0.90% 0.01
Fe2O3 0.62% -
LOI 0.10%n/a
Oxide Weight 41.23
Formula Weight 41.27