Petalite Cornell

Oxide Analysis Formula Tolerance
Li2O 4.30% 0.95
Na2O 0.50% 0.05
Al2O3 17.50% 1.13
SiO2 77.00% 8.41
LOI 0.70%n/a
Oxide Weight 651.75
Formula Weight 656.34