Milwood Sand Silica

Description: FLINT

Oxide Analysis Formula Tolerance
Al2O3 0.35% 1.00
SiO2 99.40% 482.00
Fe2O3 0.04% 0.07
LOI 0.18%n/a
Oxide Weight 29,081.66
Formula Weight 29,134.10

Notes

Sieve Analysis:

% Thru: 100# 200 325 mesh
===========================
#120 Flour 88.0 64.0 44.0
#180 Flour 98.8 96.0 77.0
#200 99.9 98.0 85.0
#325 99.9 99.8 96.6
#375 99.9 99.8 98.0

Many grades and sizes of sand also available.

Related Information

Links

Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.