1 2 3 Ball Clay

Alternate Names: 123 Ball Clay

Description: Low carbon ball clay

Notes

A fine-grained engineered blend with excellent green strength and fired color. Formulated with extremely low levels of carbon and sulfur. 123 is ideally suited in fast-fired tile and dinnerware applications.

Related Information

Links

Oxide Analysis Formula Tolerance
Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.